China-Yixing Longly Refractories Shelf Boards and Pillars SiC

Category Ceramic , Carbide
Manufacturer China-Yixing Longly Refractories Co. Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China-Yixing Longly Refractories Shelf Boards and Pillars SiC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibration or hydraulic machine to suppress, high-temperature shuttle kiln firing; products performance and stability excellent, thermal shock good, oxidation resistance good, wear resistance excellent, heat-shock excellent, not slag off, long service life. The appearance of products formed, smooth, high-volume density, good thermal conductivity, energy-saving effect significant.Applications: Widely used in a variety of tunnel kiln, roller kiln, shuttle kiln production of sanitary ceramics, daily-use ceramics, art ceramics, magnetic materials, powder metallurgy, electrical porcelain, industrial ceramics, as well as refractory products, such as the firingInformation Provided by China Yixing Longly Refractories Co. Ltd
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.95 g/cc
0.0975 - 0.107 lb/in³
Porosity 8.0 - 9.0 %
8.0 - 9.0 %
Apparent
Mechanical Properties Metric English Comments
Flexural Strength >= 580 MPa
>= 84100 psi
cold bending
>= 650 MPa
>= 94300 psi
high temp bending
Compressive Strength >= 1200 MPa
>= 174000 psi
Ambient
Thermal Properties Metric English Comments
CTE, linear 2.20 µm/m-°C
1.22 µin/in-°F
Volumetric thermal expansion
Thermal Conductivity 15.5 - 16.5 W/m-K
108 - 115 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air >= 1450 °C
>= 2640 °F
Component Elements Properties Metric English Comments
SiC >= 89.9 %
>= 89.9 %
Descriptive Properties Value Comments
Refractoriness (°C) >1400
Under load temperature, 0.2 MPa, 0.6%
Thermal Shock Resistance Times 60
1100°C water cooling