Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.19 g/cc | 0.296 lb/in³ | |
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Deloro® N-6 PM with P/M Processing Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Latrobe DuraTechâ„¢ T15 Powder Metal High Speed Steel (ASTM T15) DuraTech T15 powder metallurgy high speed steel is cobalt-bearing super high speed steel which can be heat treated to a hardness as high as 67 Rockwell C. A high volume of hard vanadium carbides pro.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.50 inch (12.7 mm) o.d. and 0.050 inch (1.27 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.50 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.75 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® Alloy 718 Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals NIMONIC® Alloy 80A A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Williams Advanced Alloys WS174 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Jet engine rings, discs, shafts, compressor blades, seals, spacers. Fasteners, nuclear, oil & gas components. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allvac® 718-OP® UNS N07718 Nickel Superalloy Uses: Turbines and engines, fasteners, sub-surface safety valves, hot extrusion tooling, nuclear reactors.Property values are for samples in the metallurgical condition: 1800°F age.Information prov.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
AIM 70In/30Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Deloro® N-6 PM cast Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age Data provided by Allvac.Applications: Turbine compressor blades and discs, shafts, spacers, fasteners, miscellaneous jet engine hardware; space shuttle turbo pump seals.Waspaloy is a registered trad.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21) TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service .. |