Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Rolled Strip, 0.150 inch (3.81 mm) Thick. Other property values are typical of INCONEL® alloy 690.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.19 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 724 MPa
105000 psi
Tensile Strength, Yield 348 MPa

@Strain 0.200 %
50500 psi

@Strain 0.200 %
Elongation at Break 41 %
41 %
Modulus of Elasticity 211 GPa
30600 ksi
Poissons Ratio 0.289
0.289
Shear Modulus 81.8 GPa
11900 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 14.06 µm/m-°C

@Temperature 24.0 - 100 °C
7.811 µin/in-°F

@Temperature 75.2 - 212 °F
Mean
14.53 µm/m-°C

@Temperature 24.0 - 300 °C
8.072 µin/in-°F

@Temperature 75.2 - 572 °F
Mean
15.19 µm/m-°C

@Temperature 24.0 - 500 °C
8.439 µin/in-°F

@Temperature 75.2 - 932 °F
Mean
17.41 µm/m-°C

@Temperature 20.0 - 1000 °C
9.672 µin/in-°F

@Temperature 68.0 - 1830 °F
Mean, extrapolated
Specific Heat Capacity 0.450 J/g-°C
0.108 BTU/lb-°F
Thermal Conductivity 13.5 W/m-K
93.7 BTU-in/hr-ft²-°F
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Solidus 1343 °C
2449 °F
Liquidus 1377 °C
2511 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 27 - 31 %
27 - 31 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 7.0 - 11 %
7.0 - 11 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Nickel, Ni >= 58 %
>= 58 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001148 ohm-cm
0.0001148 ohm-cm
Magnetic Permeability 1.001
1.001
at 200 Oersted (15.9 kA/m)