Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness. Other property values are typical of INCONEL® alloy 690.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.19 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 648 MPa
94000 psi
Tensile Strength, Yield 282 MPa

@Strain 0.200 %
40900 psi

@Strain 0.200 %
Elongation at Break 52 %
52 %
Modulus of Elasticity 211 GPa
30600 ksi
Poissons Ratio 0.289
0.289
Shear Modulus 81.8 GPa
11900 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 14.06 µm/m-°C

@Temperature 24.0 - 100 °C
7.811 µin/in-°F

@Temperature 75.2 - 212 °F
Mean
14.53 µm/m-°C

@Temperature 24.0 - 300 °C
8.072 µin/in-°F

@Temperature 75.2 - 572 °F
Mean
15.19 µm/m-°C

@Temperature 24.0 - 500 °C
8.439 µin/in-°F

@Temperature 75.2 - 932 °F
Mean
17.41 µm/m-°C

@Temperature 20.0 - 1000 °C
9.672 µin/in-°F

@Temperature 68.0 - 1830 °F
Mean, extrapolated
Specific Heat Capacity 0.450 J/g-°C
0.108 BTU/lb-°F
Thermal Conductivity 13.5 W/m-K
93.7 BTU-in/hr-ft²-°F
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Solidus 1343 °C
2449 °F
Liquidus 1377 °C
2511 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 27 - 31 %
27 - 31 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 7.0 - 11 %
7.0 - 11 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Nickel, Ni >= 58 %
>= 58 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001148 ohm-cm
0.0001148 ohm-cm
Magnetic Permeability 1.001
1.001
at 200 Oersted (15.9 kA/m)