Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.74 - 2.06 g/cc
0.0629 - 0.0744 lb/in³
Average value: 1.83 g/cc Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim..
Density 1.95 - 2.06 g/cc
0.0704 - 0.0744 lb/in³
ASTM D792
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.
Density 2.02 - 2.06 g/cc
0.0730 - 0.0744 lb/in³
ISO R 1183
Fainplast Compounds CRKA 90 Flexible PVC, Flame Retardant Electrical Bedding Lead Free
Bedding non contaminating on XLPE
Density 0.880 - 2.06 g/cc
0.0318 - 0.0744 lb/in³
Average value: 1.37 g/cc Grade Count:1191
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..