Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Mineral/Graphite Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.74 - 2.06 g/cc
0.0629 - 0.0744 lb/in³
Average value: 1.83 g/cc Grade Count:8
Water Absorption 0.0350 - 0.0480 %
0.0350 - 0.0480 %
Average value: 0.0431 % Grade Count:8
Linear Mold Shrinkage 0.00173 - 0.00420 cm/cm
0.00173 - 0.00420 in/in
Average value: 0.00261 cm/cm Grade Count:8
Mechanical Properties Metric English Comments
Hardness, Rockwell E 58.0 - 61.0
58.0 - 61.0
Average value: 59.2 Grade Count:5
Tensile Strength, Ultimate 31.0 - 89.0 MPa
4500 - 12900 psi
Average value: 43.9 MPa Grade Count:8
Elongation at Break 0.236 - 0.580 %
0.236 - 0.580 %
Average value: 0.399 % Grade Count:8
Modulus of Elasticity 10.3 - 29.0 GPa
1490 - 4210 ksi
Average value: 15.2 GPa Grade Count:8
Flexural Yield Strength 55.0 - 163 MPa
7980 - 23600 psi
Average value: 76.3 MPa Grade Count:8
Flexural Modulus 10.0 - 26.0 GPa
1450 - 3770 ksi
Average value: 13.3 GPa Grade Count:8
Compressive Yield Strength 117 - 269 MPa
17000 - 39000 psi
Average value: 151 MPa Grade Count:8
Izod Impact, Notched 0.156 - 0.174 J/cm
0.292 - 0.326 ft-lb/in
Average value: 0.163 J/cm Grade Count:7
Charpy Impact, Notched 0.144 - 0.260 J/cm²
0.685 - 1.24 ft-lb/in²
Average value: 0.178 J/cm² Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 32.0 - 38.0 µm/m-°C

@Temperature 40.0 - 130 °C
17.8 - 21.1 µin/in-°F

@Temperature 104 - 266 °F
Average value: 34.0 µm/m-°C Grade Count:3
Thermal Conductivity 1.22 - 1.94 W/m-K

@Temperature 100 - 100 °C
8.47 - 13.5 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 1.58 W/m-K Grade Count:2
Maximum Service Temperature, Air 200 - 257 °C
392 - 495 °F
Average value: 220 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 180 - 222 °C
356 - 432 °F
Average value: 193 °C Grade Count:8
Copyright © lookpolymers.com All Rights Reserved