Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.880 g/cc | 0.0318 lb/in³ | STN EN ISO 1183-1 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | STN 64 0111 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Density | 0.880 - 1.62 g/cc | 0.0318 - 0.0585 lb/in³ | Average value: 1.34 g/cc Grade Count:85 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 0.880 - 0.960 g/cc | 0.0318 - 0.0347 lb/in³ | Average value: 0.924 g/cc Grade Count:71 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | d20/20 |
Mitsui UNISTOLEâ„¢ P-901 Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ P is a liquid primer for coating and bonding polypropylene (PP) and various engineering plastics, rubber and other materials, which do not readily bond. Characteristics An easily han.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA 10 A is a thermoplastic polyolefin which has been developed for the extrusion and calendering of soft film and sheet. Thanks to its high rubber content "Hifax" CA 10 A fe.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
Silon Tabond 2003 Adhesive Resin TABOND 2003 is a ethylene-octene copolymer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT318 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ISO 1183 |
Polyram Bondyram® 7103 Maleic Anhydride Modified Ethylene-Alpha Olefin Copolymer High flow impact modified for Nylon compounds un-reinforced and glass fiber reinforced. Good retention of impact at low temperatures.Information provided by Polyram. |
|||
Density | 0.880 g/cc @Temperature 15.0 °C |
0.0318 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Heavy Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 55 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Density | 0.880 g/cc @Temperature 15.6 °C |
0.0318 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 1500 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D297 |
Dow Nordel® IP 3720P EPDM Hydrocarbon Rubber Description: This semicrystalline, very low diene containing ethylene-propylene terpolymer (EPDM) has a low viscosity for excellent processing characteristics and low unsaturation for stability duri.. |