Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Viscosity Measurement 0.98 - 1.02
0.98 - 1.02
[dl/g]; ASTM D2857
Melt Index of Compound 25 - 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
25 - 31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
ASTM Color -2.50 - 0.50
-2.50 - 0.50
[a Value]; JIS Z8722
-2.00 - 2.0
-2.00 - 2.0
[b Value]; JIS Z8722
81 - 87
81 - 87
[L Value]; JIS Z8722
Thermal Properties Metric English Comments
Melting Point >= 220 °C
>= 428 °F
ASTM D3418
Chemical Properties Metric English Comments
Acid Value <= 40
<= 40
[µ equ/g]; Zimmer PV07013.4
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
ASTM D4019
Descriptive Properties Value Comments
THF Content, ppm <2000
Gas Chromatography