Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.939 g/cc | 0.0339 lb/in³ | Compression Molded; ASTM D792 |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
SABIC R40039E Medium Density Polyethylene for Rotational Molding Product Description: R40039E is a Medium Density Polyethylene grade designed to provide excellent mechanical properties with high rigidity, toughness, gloss and low warpage. R40039E is UV stabiliz.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L63935U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsFormolene L63935U is fully heat and UV stabilized.Meets all requirements of the U.S. Food and Drug Adminis.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D792 |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D 792 |
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **) Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8504 UV8D, 8504G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 155-1330 LMDPE Rotational Molding Resin Description: ICORENE 155-1330 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Density | 0.939 g/cc @Temperature 20.0 °C |
0.0339 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell Glycol Ether EBA Ethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 3802 FA HDPE Film Applications:General purpose thin film, trash bags, merchant bagsBlending partnerFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 10D neck height.Information provi.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D-1505 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ LD 730.09 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 730.09 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: Latin America, North Amer.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | natural resin; ASTM D792 |
Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM-D1505 |
Braskem ML4400N LLDPE Rotomolding Polyethylene The resin ML4400N is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long t.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM-D1505 |
Braskem RC35U4 LLDPE Rotomolding Polyethylene The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM-D729 |
Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer IN34 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibil.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Base Density |
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Density | 0.939 - 0.970 g/cc | 0.0339 - 0.0350 lb/in³ | Average value: 0.951 g/cc Grade Count:130 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |