Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® 3802N Natural HDPE pipe grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® 3802N Natural HDPE pipe grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D 792
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
PENT >= 5000 hour
>= 5000 hour
ASTM F 1473
Hardness, Shore D 65
65
ASTM D 2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D 638 type IV
Tensile Strength, Yield >= 17.9 MPa
>= 2600 psi
ASTM D 638 type IV
Elongation at Break >= 700 %
>= 700 %
ASTM D 638 type IV
Flexural Modulus 0.703 GPa
102 ksi
ASTM D 790
Hydrostatic Design Basis 8.62 MPa

@Temperature 23.0 °C
1250 psi

@Temperature 73.4 °F
ASTM D 2837
Thermal Properties Metric English Comments
CTE, linear 216 µm/m-°C

@Temperature 20.0 °C
120 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 126 °C
259 °F
ASTM D3417
Vicat Softening Point 127 °C
260 °F
ISO 306
Users viewing this material also viewed the following: