ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Exxon Chemical
Trade Name Escor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide films, metalized films, papers, iron steel and glass. Very high bond resistance even for acidic and aggressive food products. Very low sealing and hot tack initiation temperature, very high hot tack peak force.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications:Aluminum Containing PackagingCoextrusion Coating Extrusion CoatingExtrusion LaminationFood packaging Metalized Films Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ExxonMobil method
Acrylic Acid Content 11 %
11 %
ExxonMobil Method
Melt Flow 14 g/10 min
14 g/10 min
ASTM D1238
Neck In 6.86 cm

@Temperature 280 °C
2.70 in

@Temperature 536 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
14.2 cm

@Temperature 280 °C
5.60 in

@Temperature 536 °F
164 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 6.33 m/s
1250 ft/min
Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point <= 201 °C
<= 394 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 71.1 °C
160 °F
ASTM D1525