Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging applications. When blended with yellow concentrate, this resin meets ASTM D3350-99 Class 234363E; PPI Recommended Designation PE 2406; and is not recommended for food applications.Characteristics: outstanding resistance to slow crack growth, contains UV stabilizer, outstanding pipe ring ESCR Applications: pipe for gas distribution, oil field and other industrial pipeData provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 5000 hour
>= 5000 hour
Cond. A, B, and C; 100% Igepal®; F<sub>50</sub>; ASTM D1693
>= 5000 hour
>= 5000 hour
Pipe Ring; ASTM F1278
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 g/10 min

@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
Mechanical Properties Metric English Comments
PENT >= 1000 hour
>= 1000 hour
ASTM F1473
Tensile Strength at Break 33.1 MPa
4800 psi
Type IV; 50 mm per min; ASTM D638
Tensile Strength, Yield 19.3 MPa
2800 psi
Type IV; 50 mm per min; ASTM D638
Elongation at Break >= 500 %
>= 500 %
Type IV; 50 mm per min; ASTM D638
Flexural Modulus 0.621 GPa
90.0 ksi
ASTM D3350
0.758 GPa
110 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 193 - 216 °C
379 - 421 °F
Stock