Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IN34 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibility, and low warpage. It was specially developed for lids fast-cycle molding injection, natural color and dyed for food. It is also recommended for the food market. IN34 was developed to be injected in similar conditions to low-density polyethylene of similar fluidity. Recommended temperature profile: 170º to 210 ºC.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM-D729
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 190 °C
48 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM-D2240
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM-D638
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM-D638
Elongation at Break 100 %
100 %
ASTM-D638
Elongation at Yield 12 %
12 %
ASTM-D638
Modulus of Rigidity 0.645 GPa
93.6 ksi
ASTM-D747
Flexural Modulus, 1% Secant 640 MPa
92800 psi
ASTM-D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °C
120 °F
ASTM-D648
Vicat Softening Point 100 °C

@Load 1.02 kg
212 °F

@Load 2.25 lb
ASTM-D1525