Physical Properties Metric English Comments
Density 0.921 - 0.970 g/cc
0.0333 - 0.0350 lb/in³
Average value: 0.931 g/cc Grade Count:191
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Density 0.945 - 0.970 g/cc
0.0341 - 0.0350 lb/in³
ASTM D792
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE
Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®.
Density 0.964 - 0.969 g/cc
0.0348 - 0.0350 lb/in³
ASTM D4052
ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaInformation provided by ExxonMobil
Density 0.965 - 0.970 g/cc
0.0349 - 0.0350 lb/in³
BRCP 4843
ExxonMobil Jayflex™ DIDP Plasticizer
Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil
Density 0.964 - 0.968 g/cc
0.0348 - 0.0350 lb/in³
ASTM D4052
ExxonMobil Jayflex™ DIDP Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaCAS Number: 68515-49-1EC Number: 271-091-4Information provided by ExxonMobil
Density 0.965 - 0.970 g/cc
0.0349 - 0.0350 lb/in³
BRCP 4843
ExxonMobil Jayflex™ DIDP-E Plasticizer
Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil
Density 0.960 - 0.970 g/cc

@Temperature 20.0 °C
0.0347 - 0.0350 lb/in³

@Temperature 68.0 °F
Oceanchem Group Tri-isobutyl Phosphate (TIBP)
Molecular Formula: C12H27O4PCas No.: 126-71-6Chemical Properties: Ester property, it can be hydrolyzed in basic condition.Hazardous Features: It can be fired in heat, fire and oxidation condition, a..
Density 0.939 - 0.970 g/cc
0.0339 - 0.0350 lb/in³
Average value: 0.951 g/cc Grade Count:130
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Density 0.940 - 0.970 g/cc
0.0340 - 0.0350 lb/in³
Average value: 0.957 g/cc Grade Count:48
Overview of materials for Ionomer, Molded