Physical Properties Metric English Comments
Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
ASTM D792
Polikim EFALON® C-25 PTFE, 25% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Pyrotek Bonded Particle Filtration Media
Bonded particle filtration media is a proven and efficient means for removing oxides from molten aluminum and its alloys. This filtration media is available in either high strength alumina oxide or..
Density 2.00 - 2.30 g/cc
0.0723 - 0.0831 lb/in³
Average value: 2.16 g/cc Grade Count:35
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
molded; ASTM D792
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon®
Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
Mo-Sci Corporation GL-0261 Ni Coated Borosilicate Glass Spheres
Appearance: Solid borosilicate glass microspheres with metallic nickel coatingTypical applications of GL-0261 glass microspheres include: conductive filler for plastic, pigment, and etc.Information ..
Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres
Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information ..
Density 2.15 - 2.30 g/cc
0.0777 - 0.0831 lb/in³
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.15 - 2.30 g/cc
0.0777 - 0.0831 lb/in³
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled
White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol..
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Beijing Evergrow Resources PTFE Gasket
PTFE gasket is manufactured by molding method with PTFE granular resin. PTFE compared with other plastics, has a superior properties against chemicals and temperature. Because of such excellent prop..
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
apparent
Beijing Evergrow Resources PTFE Tube and Pipe
PTFE tubing is manufactured by ram extruding method with PTFE granular resin. It has good electrical properties.Information provided by Beijing Evergrow Resources.
Density 1.85 - 2.30 g/cc
0.0668 - 0.0831 lb/in³
Compounded
Fluorocarbon Rubber (FPM), Low Temperature Grade
Fluorocarbon rubbers are very stable toward degradation by chemicals, heat, and oxidation. Some chemicals that attack FPM include ketones, low molecular weight esters, and nitrogen containing solve..
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Beijing Evergrow Resources PTFE Skived Sheet Tape
PTFE resin is first molded into work-blank and then skived. The PTFE resin skived sheet & tape are highly dielectric. Chemical resistant and not aging. They have a wide range of operation temperatur..