Physical Properties Metric English Comments
Density 2.20 - 2.50 g/cc
0.0795 - 0.0903 lb/in³
ASTM B212
H.C. Starck Amperit® 827.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
Density 1.60 - 2.50 g/cc
0.0578 - 0.0903 lb/in³
Sibur VO Compound VNP Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Density 2.10 - 2.50 g/cc
0.0759 - 0.0903 lb/in³
Du-Co Ceramics DC-187 Magnesium Oxide
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Density 0.550 - 2.50 g/cc
0.0199 - 0.0903 lb/in³
Average value: 1.29 g/cc Grade Count:568
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Density 1.03 - 2.50 g/cc
0.0372 - 0.0903 lb/in³
Average value: 1.11 g/cc Grade Count:25
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..