Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.801 - 1.52 g/cc | 0.0289 - 0.0549 lb/in³ | Average value: 1.30 g/cc Grade Count:53 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.37 - 1.52 g/cc | 0.0495 - 0.0549 lb/in³ | Average value: 1.47 g/cc Grade Count:6 |
Overview of materials for Silicone, RTV, Construction Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 265/D Rigid PVC, Extrusion Semi-rigid furniture border |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 88/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 80 Flexible PVC, Sheathing General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 85 Flexible PVC, Flame Retardant Insulation Lead Free Power cables |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 86 Flexible PVC, Insulation General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 75/3 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 86/2 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/13 Halogen Free PVC General purpose |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/33 Halogen Free PVC Sheathing, high flexibility |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 045/11 Halogen Free PVC Sheathing; designed to meet VDE 0207 part 24 HM4 |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 20 Halogen Free PVC Sheathing; Insulation, low cost for general purpose |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 22G Halogen Free PVC Sheathing; standard grade improved processing speed |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3522D Halogen Free PVC Sheathing; standard grade improved processing speed |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 36/O Halogen Free PVC General purpose |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3622 Halogen Free PVC General purpose |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3821 Halogen Free PVC Sheathing, high flexibility |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 417 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:SheathingInformation provided by Fainplast Compounds |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1184 |
Fainplast Compounds R 211 Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 4024 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Density | 1.43 - 1.52 g/cc | 0.0517 - 0.0549 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.19 - 1.52 g/cc | 0.0430 - 0.0549 lb/in³ | Average value: 1.31 g/cc Grade Count:8 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.31 - 1.52 g/cc | 0.0473 - 0.0549 lb/in³ | Average value: 1.41 g/cc Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 92 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 045/11 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 80/A Flexible PVC, Lead Free Pipes and profiles |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 50/C Flexible PVC, Extrusion Gaskets for frames |
|||
Density | 1.05 - 1.52 g/cc | 0.0379 - 0.0549 lb/in³ | Average value: 1.16 g/cc Grade Count:102 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |