Fainplast Compounds GK 86/2 Flexible PVC, Flame Retardant Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GK 86/2 Flexible PVC, Flame Retardant Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.48 - 1.52 g/cc
0.0535 - 0.0549 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 89
85 - 89
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 240 %
>= 240 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 32.5 %
32.5 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 35
CEI 20-34/3-2