Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2020 LO-GC Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2797 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging RB-FG Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® RB-FG is a clear, rigid PVC compound designed specifically for use as a color/ stability booster additive in Geon® packaging compounds where high regrind usage is necessary in extrusion blow.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging VEO-111 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | |
Pyrotek Pyrite N-17 Refractory Board Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | |
Pyrotek Wollite 50 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Density | 0.801 - 1.52 g/cc | 0.0289 - 0.0549 lb/in³ | Average value: 1.30 g/cc Grade Count:53 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.801 - 1.36 g/cc | 0.0289 - 0.0491 lb/in³ | Average value: 1.22 g/cc Grade Count:123 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Unifrax Fiberfrax® LDS Moldable Moldable Insulation Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Unifrax Fiberfrax® Pumpable-LDS Pumpable Insulation Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have te.. |
|||
Density | 0.801 - 0.961 g/cc | 0.0289 - 0.0347 lb/in³ | Dry |
Unifrax Fiberfrax® Vari-Form™ B Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Density | 0.801 - 0.961 g/cc | 0.0289 - 0.0347 lb/in³ | |
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM C134 |
BNZ Materials BNZ-26-60 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |