Material Notes:
Formula: C2H6OSCAS: 60-24-2Description: Mercaptoethanol is a colorless to yellow liquid, with an amine-like odor. It is also miscible with water.Synonyms: Monothioglycol, 2-Hydroxy-1-ethanethiol, 2-Hydroxyethanethiol, 2-Mercaptoethyl alcohol, Thiomonoglycol, Thioethylene glycolApplications: Intermediate used in the production of PVC stabilizer, Crop protection, Pharmaceuticals, Photographic chemicals, Solvent and stabilizer, Initial product for chemical syntheses and Corrosion InhibitorInformation provided by BASF
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Molecular Weight 78.1 g/mol
78.1 g/mol
Thermal Properties Metric English Comments
Melting Point <= -50.0 °C
<= -58.0 °F
Boiling Point 154 - 161 °C
309 - 322 °F
Flash Point 68.0 °C
154 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN ISO 3733
Descriptive Properties Value Comments
Assay >99%
Color <20
APHA, DIN ISO 6271
Composition Dithiodiglycol
<0.25%
Thiodigylcol
<0.25%
Ignition Temperature 295°C