Material Notes:
Key Features: medium high melt flow, very high modulus, UV-stabilized, mineral-filled polypropylene copolymer, very high rigidity, good impact resistance, good weatherability, good processabilityApplications: cowl net grillesDescription: Astyrn EPKC10ZC medium high melt flow, UV-stabilized, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness, impact resistance, weatherabiiity and processability. It was designed primarily for automotive exterior applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ISO 2577
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO R527
Elongation at Yield 5.0 %
5.0 %
ISO R527
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Izod Impact, Notched 3.90 J/cm

@Temperature 23.0 °C
7.31 ft-lb/in

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
ISO 75