Material Notes:
Film Grade. Nylene 615 is an extrusion grade nylon 6 resin suitable for coating and film co-extrusion applications. It has excellent melt stability and good melt strength. Nylene 615 has superior grease resistance, toughness, resistance to abrasion, and does not absorb food odors. Nylene 15 meets the requirements of FDA regulation 21 CFR 177.1500 for direct food contact.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 38.0 MPa
5510 psi
Orientation not specified; ASTM D882
Film Elongation at Break, MD 290 %
290 %
Orientation not specified; ASTM D882
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Elmendorf Tear Strength MD 56 g
56 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 60.0 MPa
8700 psi
Orientation not specified; ASTM D882