Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BG373MO Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BG373MO Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BG373MO is a heterophasic copolymer. Products molded with this grade exhibit excellent antistatic performance and very good mould release. Electrostatic charge is
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ISO 2309-2
Tensile Strength, Yield 27.0 MPa
3920 psi
50mm/min; ISO 527-2
Elongation at Yield 5.0 %
5.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.55 GPa
225 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 20.0 J

@Temperature -20.0 °C
14.8 ft-lb

@Temperature -4.00 °F
ISO 6603-2
24.0 J

@Temperature 0.000 °C
17.7 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity highest possible