PolyOne Syncure™ S1042A Polyethylene, Crosslinked (XLPE)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer PolyOne Corporation
Trade Name Syncure™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Syncure™ S1042A Polyethylene, Crosslinked (XLPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Deformation, and Gel measured on a 95 phr S1042A / 5 phr S1000B system; and cured for 6 hours in water at 90 degree C. Brittleness Temperature isInformation provided by PolyOne
Physical Properties Metric English Comments
Density 0.490 g/cc
0.0177 lb/in³
Geon® 1169; Internal Method
0.912 g/cc
0.0329 lb/in³
ASTM D1505
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Deformation 5.0 %

@Temperature 131 °C,
Time 3600 sec
5.0 %

@Temperature 268 °F,
Time 1.00 hour
500 g; UL 1581
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.1 MPa
1900 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -70.0 °C
-94.0 °F
ASTM D746
Descriptive Properties Value Comments
Appearance Pellets/Cubes
ASTM D2090
Forms Pellets
Gel Content 75%
ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic Material XLPE
Generic Name Polyethylene, Crosslinked (XLPE)
Regional Availability North America
Uses Wire & Cable Applications