Solvay TECHNYL® 1021ST PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 1021ST PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balanced mechanical properties. It is suitable for all sectors industries such as: Bowling pin, Brake drum, Inline skate part. This product is available natural colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 1.2 %

@Temperature 23.0 °C,
Time 86400 sec
1.2 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D786
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 11.0 J/cm
20.6 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Flammability, UL94 HB
HB
ISO 1210
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.5
3.5
IEC60250
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 235 - 240 °C
455 - 464 °F
Front Barrel Temperature 250 - 260 °C
482 - 500 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 245-350°C