Lucas-Milhaupt Clean & Bright & Brite Tin/ Silver Solder

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Lucas-Milhaupt
Trade Name Clean & Bright
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Clean & Bright & Brite Tin/ Silver Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the proper flux will wet stainless very well. Sn96 is the eutetic composition, is very fluid, and will not bridge large gaps.. Joint clearances of 0.1 to 0.15mm (.003 to .005 in) are optimum, but larger variations can still produce sound joints. Flux is required and proper selection will depend upon base metals to be joined.Specifications:This alloy conforms to the following specification: ASTM B32-Sn96 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 7.355 g/cc
0.2657 lb/in³
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
Solidus 221 °C
430 °F
Melting Point
Liquidus 221 °C
430 °F
Flow Point
Component Elements Properties Metric English Comments
Silver, Ag 3.5 %
3.5 %
Tin, Sn 96.5 %
96.5 %
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: