| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® VR2520 PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D 792 |
| Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D 792 |
| 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 | |
| Water Absorption | 0.15 % <br>@Time 86400 sec |
0.15 % <br>@Time 24.0 hour |
ASTM D 570 |
| Moisture Absorption at Equilibrium | 0.15 % | 0.15 % | 23°C / 50% RH; ISO 62 |
| 0.35 % <br>@Temperature 23.0 °C |
0.35 % <br>@Temperature 73.4 °F |
ASTM D 570 | |
| 0.58 % <br>@Temperature 100 °C |
0.58 % <br>@Temperature 212 °F |
ASTM D 570 | |
| Water Absorption at Saturation | 0.35 % <br>@Temperature 23.0 °C |
0.35 % <br>@Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 8.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
8.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| 8.5 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
8.5 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D 638 |
| 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D 638 |
| 63.0 MPa | 9140 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 110 % | 110 % | 50 mm/min; ISO 527 |
| 130 % | 130 % | Type I, 50 mm/min; ASTM D 638 | |
| Elongation at Yield | 6.0 % | 6.0 % | 50 mm/min; ISO 527 |
| 7.0 % | 7.0 % | Type I, 50 mm/min; ASTM D 638 | |
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 90.0 MPa | 13100 psi | 2 mm/min; ISO 178 |
| 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
| 2.34 GPa | 339 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Izod Impact, Notched | 8.01 J/cm <br>@Temperature 23.0 °C |
15.0 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D 256 |
| Izod Impact, Unnotched | 32.04 J/cm <br>@Temperature 23.0 °C |
60.02 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D 4812 |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² <br>@Temperature -30.0 °C |
4.76 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 12.0 kJ/m² <br>@Temperature 23.0 °C |
5.71 ft-lb/in² <br>@Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact Unnotched | NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| Impact Test | 63.0 J <br>@Temperature 23.0 °C |
46.5 ft-lb <br>@Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C <br>@Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F <br>@Temperature -40.0 - 203 °F |
ASTM E 831 |
| 70.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 68.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 137 °C <br>@Thickness 6.40 mm |
279 °F <br>@Thickness 0.252 in |
unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 125 °C | 257 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 132 °C <br>@Thickness 6.40 mm |
270 °F <br>@Thickness 0.252 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
| 142 °C | 288 °F | Rate B/120; ISO 306 | |
| 154 °C | 309 °F | Rate B/50; ASTM D 1525 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.586 | 1.586 | ASTM D 542 |
| Haze | 1.0 % <br>@Thickness 2.54 mm |
1.0 % <br>@Thickness 0.100 in |
ASTM D 1003 |
| Transmission, Visible | 88 % <br>@Thickness 2.54 mm |
88 % <br>@Thickness 0.100 in |
ASTM D 1003 |