Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction: Interleave: FEP FilmSide 1: Cured Silicone Rubber Carrier: PTFE Coated FiberglassProduct Use: Adhesive. Bonds without primer.Appearance: Off-white, High viscosity gum on release linersThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Interleave
76.2 microns
3.00 mil
Carrier; Arlon SQA-TMS-003
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
203 microns
8.00 mil
Side 1; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Silicone Property; ASTM D2240
Tensile Strength 6.37 MPa
924 psi
Silicone Property; ASTM D412
Elongation at Break 352 %
352 %
Silicone Property; ASTM D412
Tear Strength 15.6 kN/m
89.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 52.17 kV/mm
1325 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Natural
Total Product Weight (oz/yd2) 7.5
Arlon SQA-TMS-025