| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % <br>@Time 86400 sec |
0.30 % <br>@Time 24.0 hour |
ISO 62-1 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 23 g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C |
23 g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | Type I, 5 mm/min; ASTM D638 |
| Elongation at Break | 100 % | 100 % | Type I, 5 mm/min; ASTM D638 |
| Flexural Yield Strength | 86.0 MPa | 12500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 6.80 J/cm | 12.7 ft-lb/in | ASTM D256 |
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 4.50 J/cm² <br>@Temperature -30.0 °C |
21.4 ft-lb/in² <br>@Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 55.0 J <br>@Temperature 23.0 °C |
40.6 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| 65.0 J <br>@Temperature -30.0 °C |
47.9 ft-lb <br>@Temperature -22.0 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 128 °C <br>@Thickness 3.20 mm |
262 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 108 °C <br>@Thickness 3.20 mm |
226 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ASTM D1525 |
| 130 °C | 266 °F | Rate B/120; ISO 306 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+16 ohm | >= 1.00e+16 ohm | ROA; IEC 60093 |
| Dielectric Strength | 17.0 kV/mm <br>@Thickness 3.20 mm |
432 kV/in <br>@Thickness 0.126 in |
in oil; IEC 60243-1 |
| 25.0 kV/mm <br>@Thickness 1.60 mm |
635 kV/in <br>@Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 39.0 kV/mm <br>@Thickness 0.800 mm |
991 kV/in <br>@Thickness 0.0315 in |
in oil; IEC 60243-1 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |