Mechanical Properties Metric English Comments
Flexural Modulus 17.0 - 20.0 GPa
2470 - 2900 ksi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Resinoid 1382 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Resinoid 7051 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9..
Flexural Modulus 17.0 GPa
2470 ksi
Cookson Group Plaskon® 1002 Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea..
Flexural Modulus 17.0 GPa
2470 ksi
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A flame retardant, novolac-hardened epoxy molding compound recommended for semiconductor packages that are not stress sensitive.
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-7-120NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance moldi..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using..
Flexural Modulus 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Flexural Modulus 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Flexural Modulus 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Flexural Modulus 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Flexural Modulus 17.0 GPa
2470 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP JCL36 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JCL36 is a compound based on Polyethersulfone resin containing Carbon Fiber, PTFE. Added features include : Internally Lubricated, Electrically Conductive.
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific)
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66
LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY
Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
Vyncolit X640 Resole Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Modulus 17.0 - 22.0 GPa
2470 - 3190 ksi
Longitudinal
Goodfellow Polyaramid/Vinylester Composite Tube or Rod
Information provided by Goodfellow.
Flexural Modulus 17.0 GPa
2470 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
55% Glass Reinforced PPA High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers
Flexural Modulus 17.0 GPa
2470 ksi
transverse; ISO 178
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound
Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f..
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific)
LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber.
Flexural Modulus 17.0 GPa
2470 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.