Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0015 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
0.0015 - 0.0030 in/in
Polymerization Shrinkage
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
0.0015 - 0.0030 in/in
Polymerization Shrinkage
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cm
0.0015 - 0.0035 in/in
Polymerization Shrinkage
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Linear Mold Shrinkage 0.0015 - 0.0045 cm/cm
0.0015 - 0.0045 in/in
ISO 2577
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm
0.0015 - 0.0020 in/in
ASTM D955
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinu
Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ATM D955
Plenco 51335 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information ..
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ISO 2577
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP
BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ISO 2577
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP
SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands ..
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic
RXÂ 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
ISO 294-4
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: ..
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cm
0.0015 - 0.0035 in/in
Compression Molding. ASTM D955
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
0.0015 - 0.0030 in/in
ASTM D955
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac
FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In..
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
normal; ISO 294-4,2577
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled
Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, lo..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Injection Molding; ISO 2577
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group
Linear Mold Shrinkage 0.0015 cm/cm

@Thickness 4.00 mm
0.0015 in/in

@Thickness 0.157 in
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Linear Mold Shrinkage 0.0015 cm/cm

@Thickness 4.00 mm
0.0015 in/in

@Thickness 0.157 in
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm
0.0015 - 0.0020 in/in
ASTM D955
Diamond Polymers DIAMALOY 1001 CF20 20% Carbon Fiber Filled ABS
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap..
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene
DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman.
Linear Mold Shrinkage 0.0015 - 0.0070 cm/cm
0.0015 - 0.0070 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Linear Mold Shrinkage 0.0015 - 0.0070 cm/cm
0.0015 - 0.0070 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..