3M Dyneon™ TF 1641 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 1641 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery good surface quality of isostatic moldingsExcellent for small partsInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
@ 23°C, Sintering Molding; ASTM D4894-98a
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894-98a
Particle Size 450 µm
450 µm
average; ASTM D4894-98a
Deformation 11 %
11 %
2175 psi - permanent, 23°C, Sintering Molding; ASTM D621
15 %
15 %
2175 psi - 24 hrs, 23°C, Sintering Molding; ASTM D621
17 %
17 %
2175 psi - 100 hrs, 23°C, Sintering Molding; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 27.58 MPa
>= 4000 psi
Sintered Molding; ASTM D4894-98a
Elongation at Break 350 %
350 %
Sintered Molding; ASTM D4894-98a
Tensile Modulus 0.600 GPa
87.0 ksi
Sintered Molding; ASTM D638
Thermal Properties Metric English Comments
Melting Point 317 - 337 °C
603 - 639 °F
second; ASTM D4894-98a
332 - 352 °C
630 - 666 °F
initial; ASTM D4894-98a
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-330 °F
Flammability, UL94 V-0
V-0
Shrinkage 2.80 %

@Temperature 23.0 °C
2.80 %

@Temperature 73.4 °F
Sintering Moldings; ASTM D4894-98a
Electrical Properties Metric English Comments
Dielectric Strength 98.4 kV/mm
2500 kV/in
ASTM D149-95a