Polymer Property : Arc Resistance = 180 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 180 - 240 sec
180 - 240 sec
DIN VDE 0303
Polikim ULPOLEN® 1000 UHMWPE, UV, Antistatic
In tough operating conditions and under direct sunlight, standard Ulpolen® 1000 shows signs of wear and abrasion within a period shorter than a year. It accumulates static electric during daily use..
Arc Resistance 180 sec
180 sec
ASTM D495
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Arc Resistance 180 sec
180 sec
ASTM D495
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Arc Resistance 180 sec
180 sec
ASTM D495
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Arc Resistance 180 sec
180 sec
ASTM D495
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Arc Resistance 180 sec
180 sec
ASTM D495
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Arc Resistance 180 sec
180 sec
Pyrotek TS-114 Thermoset Electrical Insulation Product (Nema Grade: GPO-3)
Glass reinforcement, Polyester resin, Red color. Flame retardant. Excellent arc and track resistance. UL recognized.Information provided by Pyrotek.
Arc Resistance 180 sec
180 sec
ASTM D495
G-3 Fiberglass Phenolic Laminate Sheet
This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of ..
Arc Resistance 180 sec
180 sec
ASTM D495
Haysite 30000 Polyester BMC, 15% Glass Reinforced
Haysite 30000 series bulk molding compound is a general purpose material. This compound can be compression, transfer, or injection molded. This material has good mechanical properties and can be pig..
Arc Resistance 180 sec
180 sec
ASTM D495
Sumitomo Bakelite North America E 8701A Short Glass Fiber Reinforced Epoxy
E 8701A is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North Amer..
Arc Resistance 180 - 240 sec
180 - 240 sec
UL 746A
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
Arc Resistance 180 sec
180 sec
ASTM D495
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Arc Resistance 180 sec
180 sec
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 180 sec
180 sec
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Arc Resistance >= 180 sec
>= 180 sec
IPC TM-650 2.5.1
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs
For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance..
Arc Resistance >= 180 sec
>= 180 sec
D48/50; ASTM D495
Arlon AD600 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Ceramic Filled High Dielectric ConstantMechanically Robust; replaces brittle laminates that cannot withstand processing, impact or High G forcesLarge Panel SizesHigh Peel Strength for Narrow LinesBe..
Arc Resistance 180 sec
180 sec
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd
BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex..
Arc Resistance >= 180 sec
>= 180 sec
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound
BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An..
Arc Resistance 180 - 190 sec
180 - 190 sec
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Arc Resistance 180 sec
180 sec
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap..
Arc Resistance 180 - 240 sec
180 - 240 sec
ASTM D495
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Arc Resistance 180 sec
180 sec
ASTM D495
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac
FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ..
Arc Resistance 180 sec
180 sec
ASTM D495
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic
FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North..
Arc Resistance 180 sec
180 sec
ASTM D495
Sumitomo Bakelite North America RX® 852 Novolac Phenolic
Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group
Arc Resistance 180 sec
180 sec
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 180 sec
180 sec
Cookson Group Plaskon® 3300S Mineral Filled Novolac Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, flame retardant, novolac hardened epoxy molding compound designed to provide hermeticity protection exceeding that ..