| Category | Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Stat-Tech™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | <= 0.00010 cm/cm | <= 0.00010 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 103 MPa | 14900 psi | ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| Tensile Modulus | 15.2 GPa | 2200 ksi | ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
| Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | <= 100 ohm-cm | <= 100 ohm-cm | ASTM D257 |
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 316 - 343 °C | 601 - 649 °F | |
| Mold Temperature | 135 - 149 °C | 275 - 300 °F | |
| Drying Temperature | 135 - 149 °C | 275 - 300 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Electrically Conductive | |
| Electromagnetic Shielding (EMI) | ||
| Radio Frequency Shielding (RFI) | ||
| Forms | Pellets | |
| Generic Material | LCP | |
| Generic Name | Liquid Crystal Polymer (LCP) | |
| Processing Method | Injection Molding | |
| Regional Availability | North America |