Mechanical Properties Metric English Comments
Izod Impact, Notched 2.40 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
4.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ NI-30CF/15T-2S Polyamide 610 (Nylon 610)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D-256
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Nylene® Norpex® AX245 PPE (Polyphenylene Ether)
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Nylene® PA6/6 Impact Modified 311 HS Nylon 6/6
Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
Izod Impact, Notched 2.40 J/cm

@Temperature -30.0 °C
4.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® BFL4000U PC
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm
4.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin  (discontinued **)
Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc..
Izod Impact, Notched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
Izod Impact, Notched 2.40 J/cm

@Temperature 22.8 °C
4.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Spartech PP7130 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Izod Impact, Notched 2.40 - 2.94 J/cm

@Thickness 3.17 mm
4.50 - 5.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman 710H Utility Black ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Izod Impact, Notched 2.40 - 2.94 J/cm

@Thickness 3.17 mm
4.50 - 5.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman 730H White ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific)
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 357HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 2.40 J/cm

@Temperature 22.8 °C
4.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Sinpolene GPP5620 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; ..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene
DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 2.40 J/cm

@Temperature -40.0 °C
4.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABS 2501 Injection Molding Grade, Medium Impact, High Flow
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 2.40 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
4.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (discontinue
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
Reliance Industries Reclair Crosslinked R35042
Crosslinkable R35042 is a polyethylene grade that has increased service temperature and toughness, and improved ESCR over Reclair R35042. Crosslinkable R35042 applications include fuel tanks and ch..
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene
DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 2.40 - 6.70 J/cm
4.50 - 12.6 ft-lb/in
Average value: 4.20 J/cm Grade Count:7
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..