Polymer Property : Vicat Softening Point = 214 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific)
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 101 °C
214 °F
0.125 inch bar, 1 Kg; ASTM D1525
Network Polymers SAN 277 Blue Tint Color
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Vicat Softening Point 101 °C
214 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific)
Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance..
Vicat Softening Point 101 °C
214 °F
50°C/h 50N
Ineos ABS Centrex® 815 ASA Blend  (discontinued **)
Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye..
Vicat Softening Point 101 °C
214 °F
ISO
I. Stern N2380 High Heat Crystal Polystyrene
Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St..
Vicat Softening Point 101 °C
214 °F
ASTM D1525
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)
Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig..
Vicat Softening Point 101 °C
214 °F
Rate B/120; ISO 306
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS
LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability.
Vicat Softening Point 101 °C

@Load 5.10 kg
214 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution Absolac® 120 HR ABS
High impact gradeGood flowInformation provided by Styrolution
Vicat Softening Point 101 °C
214 °F
VST/B/50; ISO 306
Styrolution Polystyrol 158 K GR 2 PS
Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati..
Vicat Softening Point 101 °C
214 °F
VST/B/50; ISO 306
Styrolution Polystyrol 158 K GR 21 PS
Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati..
Vicat Softening Point 101 °C

@Load 5.10 kg
214 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution PS 153F GPPS
Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica..
Vicat Softening Point 101 °C

@Load 1.02 kg
214 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Styrolution PS 6210/6211 HIPS
Great balance of rigidity and toughnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution
Vicat Softening Point 101 °C
214 °F
B/120; ISO R306
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 101 °C
214 °F
B/50; ISO R306
Samsung Cheil Industries Starex® SV-0157 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Vicat Softening Point 101 °C
214 °F
1kg / 120°C; ASTM D1525
Supreme Petrochem SC 203EL General Purpose Polystyrene
CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cass..
Vicat Softening Point 101 °C
214 °F
1kg / 120°C; ASTM D1525
Supreme Petrochem SP 6410 0003 Abrasion Resistant Polystyrene
Characteristics Self lubricating, abrasion resistant Low specific Gravity Suitable for multicavity thin wall parts Excellent thermal stability and easy to color Processing Injection moldingApplic..
Vicat Softening Point 101 °C
214 °F
UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Vicat Softening Point 101 °C
214 °F
50N (T° increase = 5°C/h); ISO 306B50
Total PSC 1960N Crystal Polystyrene
1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti..
Vicat Softening Point 101 °C

@Load 1.00 kg,
Thickness 3.17 mm
214 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 101 °C
214 °F
Dow AIM® 4800 High Impact Styrenic Resin
AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..
Vicat Softening Point 101 °C
214 °F
Dow Prevail® 3050 ABS + Polyurethane
PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
Vicat Softening Point 101 °C
214 °F
50N; ISO 306
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Vicat Softening Point 101 °C
214 °F
BASF Polystyrol® 168 N Polystyrene (Europe)
High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 101 °C
214 °F
BASF Polystyrol® 168 NO Polystyrene (Europe)
High molecular, heat-resistant grades for the extrusion of low-taint food packaging, especially BOPS.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 101 °C
214 °F
ASTM D1525
Americas Styrenics STYRON® 487R High Impact Polystyrene
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer..
Vicat Softening Point 101 °C
214 °F
UBE UBEPOL BR15HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBEPOL-BR15HB is characterized by the highest branching of these 3 grades and is adapted by many PS manufacturers.Information provided by UBE.
Vicat Softening Point 101 °C
214 °F
50 N - 50°C/h; ISO 306/B
Polimeri Europa Edistir N 2982 Polystyrene
General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC..