| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PPH GF1030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
| Filler Content | 30 % | 30 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | With Flow; ISO 2577 |
| 0.0070 cm/cm | 0.0070 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 85.0 MPa | <= 12300 psi | ISO/R527 |
| Elongation at Break | 4.0 % | 4.0 % | ISO/R527 |
| Flexural Strength | <= 120 MPa | <= 17400 psi | ISO 178 |
| Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.800 J/cm² @Temperature -20.0 °C |
3.81 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
| 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 125 °C @Load 5.001 kg |
257 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
| Back Pressure | 1.00 - 2.00 MPa | 145 - 290 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |