Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1010 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH DGF101015 PB Polypropylene Homopolymer, Glass Fibre/Mineral, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Melt Index of Compound | 1.0 g/10 min @Temperature 190 °C |
1.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® AT1053A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.0 g/10 min @Temperature 190 °C |
1.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® NF458A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Lushan PA+30% GF+5% AR-1A Nylon Toughener/PA Impact Modifier Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener.. |
|||
Melt Index of Compound | 1.0 - 3.0 g/10 min | 1.0 - 3.0 g/10 min | |
Sibur ABS 1106 Extrusion Grade ABS Plastic With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding .. |
|||
Melt Index of Compound | 1.0 - 3.5 g/10 min | 1.0 - 3.5 g/10 min | I Preparation |
Sibur ABS 1106M Extrusion Grade ABS Plastic With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Sibur MPP 15-06V Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8842 Polyolefin Elastomer Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle si.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube appli.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber Description: This crystalline ethylene-propylene-diene terpolymer (EPDM) has a low viscosity for excellent flow characteristics and hot green strength. It has been designed for property modification.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Arkema Group OREVAC® 18910 Maleic Anhydride Modified Copolymer OREVAC® 18910 is anhydride modified copolymer based on styrenic and ethylenic copolymers. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to proc.. |
|||
Melt Index of Compound | 1.0 - 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene OREVAC C306 is anhydride modified LLDPE. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. It has been designed.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6301Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |