| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ B70 W25 G45 H Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ±0.02 g/cm³; ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 160 MPa @Temperature 23.0 °C |
23200 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 2.0 % @Temperature 23.0 °C |
2.0 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Heat Stabilized | |
| Filler / Reinforcement | Glass Fiber Reinforcement, 45% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Processing Method | Injection Molding | |
| Regional Availability | Europe | |
| RoHS Compliance | RoHS Compliant |