Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 135 Natural Sheet Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 135 Natural Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Garlock Natural Rubber Sheet is manufactured from Food and Drug Administration-approved ingredients. It is a superior, long-life sheet designed specifically for general gasketing, countertops and skirting in all areas of food processing and pharmaceutical and cosmetics manufacturing. Approved by USDA for meat and poultry processing.Style #135 is a full-floating, natural rubber offers excellent abrasion characteristics. Also provides good resistance to most organic salts, ammonia, acids and alkalies. It is non-marking.Tan, smooth or gum finishInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength >= 20.7 MPa
>= 3000 psi
23.4 MPa
3400 psi
Typical
Elongation at Break >= 600 %
>= 600 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Compliance Properties Metric English Comments
FDA Yes
Yes
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved