Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 266 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 110 - 130 °C
230 - 266 °F
DuPont Performance Polymers Crastin® 6134 NC010 PBT  (Unverified Data**)
Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Drying Temperature 110 - 130 °C
230 - 266 °F
DuPont Performance Polymers Crastin® S620F20 BK851 PBT  (Unverified Data**)
Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly..
Drying Temperature 110 - 130 °C
230 - 266 °F
Injection Molding
DuPont Performance Polymers Crastin® SK615SF BK591 PBT  (Unverified Data**)
Crastin® SK615SF BK591 is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast ..
Drying Temperature 110 - 130 °C
230 - 266 °F
DuPont Performance Polymers Crastin® SK642FR BK851 PBT  (Unverified Data**)
Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf..
Drying Temperature 70.0 - 130 °C
158 - 266 °F
Average value: 119 °C Grade Count:88
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Drying Temperature 75.0 - 130 °C
167 - 266 °F
Average value: 95.8 °C Grade Count:8
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Latiohm 87/28-07 CNT PC
Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Latistat 87/28-06 PC
Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..
Drying Temperature 120 - 130 °C
248 - 266 °F
Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens.
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Drying Temperature 110 - 130 °C
230 - 266 °F
Injection Molding
DuPont Performance Polymers Crastin® S610SF NC010 PBT  (Unverified Data**)
Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati..
Copyright © lookpolymers.com All Rights Reserved