Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pasargad Polymer Peyvand Pasamid 3P-M2000W Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Pasargad Polymer Peyvand
Trade Name Pasamid
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Pasargad Polymer Peyvand Pasamid 3P-M2000W Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527-2
Elongation at Break 10 %
10 %
ISO 527-2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Unannealed; ISO 75-2/C
Processing Properties Metric English Comments
Rear Barrel Temperature 235 - 275 °C
455 - 527 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Descriptive Properties Value Comments
Color Black