Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Thermal Conductivity | 0.250 - 0.270 W/m-K | 1.74 - 1.87 BTU-in/hr-ft²-°F | Average value: 0.258 W/m-K Grade Count:5 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Thermal Conductivity | >= 0.250 W/m-K | >= 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0950/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 121 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Butyrate 530A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | |
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg 49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 12 Polyamide 12 This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | Average value: 0.250 W/m-K Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon 45N Multifunctional Epoxy Laminate and Prepreg Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi.. |
|||
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |