| Category | Polymer , Thermoplastic , Nylon , Nylon 612 | 
| Manufacturer | Nylacast | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Nylacast Aquanyl Nylon 612 Copolymer.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | method A; ISO 1183:1987 | 
| Water Absorption |           0.20 %                     @Time 86400 sec  | 
                  0.20 %                     @Time 24.0 hour  | 
        Immersion; ISO 62:1999 | 
| Water Absorption at Saturation | 5.0 % | 5.0 % | Immersion; ISO 62:1999 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | 78 - 82 | 78 - 82 | ISO 868:2003 | 
| Tensile Strength, Yield | 75.0 - 85.0 MPa | 10900 - 12300 psi | Type 1B, 50mm/min; ISO 527-1/2:1993 | 
| Elongation at Break | >= 20 % | >= 20 % | Type 1B, 50mm/min; ISO 527-1/2:1993 | 
| Tensile Modulus | 3.40 GPa | 493 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 | 
| Flexural Strength | 50.0 - 100 MPa | 7250 - 14500 psi | 1.5mm/min; ISO 178:2001 | 
| Flexural Modulus | 2.70 GPa | 392 ksi | 1.5mm/min; ISO 178:2001 | 
| Compressive Strength | 130 MPa | 18900 psi | Type B, 5mm/min; ISO 604:2002 | 
| Compressive Modulus | 2.60 GPa | 377 ksi | Type B, 5mm/min; ISO 604:2002 | 
| Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | Type A; ISO 180:2000 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           80.0           µm/m-°C           @Temperature 23.0 - 55.0 °C  | 
                  44.4           µin/in-°F           @Temperature 73.4 - 131 °F  | 
        ISO 11359-2:1999 | 
| Melting Point | 221 °C | 430 °F | |
| Maximum Service Temperature, Air | 160 °C | 320 °F | Intermittent | 
|           100           °C           @Time 1.80e+7 sec  | 
                  212           °F           @Time 5000 hour  | 
        Continuous | |
| Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent | 
| -40.0 °C | -40.0 °F | Continuous | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093:1980-01 | 
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093:1980-01 | 
| Dielectric Constant |           3.7                     @Frequency 1.00e+6 Hz  | 
                  3.7                     @Frequency 1.00e+6 Hz  | 
        IEC 60250:1969-01 | 
|           4.0                     @Frequency 100 Hz  | 
                  4.0                     @Frequency 100 Hz  | 
        IEC 60250:1969-01 | |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 | 
| Comparative Tracking Index | 600 V | 600 V | IEC 60112:2003-01 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Color | Natural/Yellow |