Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers OpteSTAT™ NC PC 1020 Polycarbonate based Carbon Nanotube Compound

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Ovation Polymers
Trade Name OpteSTAT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers OpteSTAT™ NC PC 1020 Polycarbonate based Carbon Nanotube Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or other electronic assemblies where ESD control is required while retaining exceptional cleanliness, dimensional control and physical propertiesAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min; ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
50 mm/min; ASTM D638
Flexural Modulus 2.65 GPa
384 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 23.0 °C
0.900 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 5000 - 1.00e+6 ohm
5000 - 1.00e+6 ohm
ASTM D257