Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 221 °C | 430 °F | ASTM D789 |
NYCOA 27/330KNF Glass Filled Nylon 6 33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Melting Point | 221 °C | 430 °F | Masterbatch; ISO 11357-1,-3 |
Nanocyl PLASTICYL™ PA1503 Polyamide 6 with 1 wt% of Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 H-TF20 Nylon 6 for injection molding, 20% PTFE lubricated Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit RECONYL B S20 Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | <= 221 °C | <= 430 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Melting Point | 221 °C | 430 °F | |
Domo Domamid® 24 Polyamide 6 DOMAMID® 24 are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo |
|||
Melting Point | 221 °C | 430 °F | |
Domo Domamid® 32 Polyamide 6 DOMAMID® 32 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization.Applications: Standard quality for production of monofilaments and fishing netsInformation pr.. |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Melting Point | 221 °C | 430 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced 40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 MK30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Melting Point | 221 °C | 430 °F | ASTM D3418 |
Ashley Polymers Ashlene® 829LF Nylon 6 Basic Nylon 6, low viscosity, lubricated. This is FDA approved.Data provided by the manufacturer |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**) Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |