Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM)

Category Polymer , Thermoplastic , Nylon
Manufacturer Mitsui Chemicals America
Trade Name Arlen™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses strong dimensional stability and chemical resistance. In addition, the effect of water absorption, which is a traditional weakness of polyamides, has been reduced to a minimum.Applications: Light-load tribological application parts of office automation equipmentInformation provided by Mitsui.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Water Absorption 0.4 %

@Thickness 2.00 mm
0.4 %

@Thickness 0.0787 in
24 hours in 23°C water; ASTM D570
2.6 %

@Thickness 2.00 mm
2.6 %

@Thickness 0.0787 in
24 hours in 100°C water; ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
Vertical Direction; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 65
65
ASTM D785
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 80.0 MPa

@Thickness 2.00 mm
11600 psi

@Thickness 0.0787 in
ASTM D638
Elongation at Break 50 %
50 %
Measured between the chucks, 2mmt; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 82.0 µm/m-°C

@Temperature 20.0 °C
45.6 µin/in-°F

@Temperature 68.0 °F
Vertical Direction; ASTM D696
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 320 °C
608 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Glass Transition Temp, Tg 125 °C
257 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
584 kV/in
ASTM D149
Dissipation Factor 0.018

@Frequency 1e+6 Hz
0.018

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Feed Temperature 50.0 - 90.0 °C
122 - 194 °F
Hopper Bottom Temp for Mechanical and Structural Standard Molding
50.0 - 90.0 °C
122 - 194 °F
Hopper Bottom for Electronic and Electric Standard Molding
Nozzle Temperature 315 - 335 °C
599 - 635 °F
NH Cylinder Temp for Electronic and Electric Standard Molding
325 - 340 °C
617 - 644 °F
NH Cylinder Temp for Mechanical and Structural Standard Molding
Zone 1 300 - 325 °C
572 - 617 °F
C1 Cylinder Temp for Electronic and Electric Standard Molding
315 - 330 °C
599 - 626 °F
C1 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 2 315 - 335 °C
599 - 635 °F
C2 Cylinder Temp for Electronic and Electric Standard Molding
320 - 335 °C
608 - 635 °F
C2 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 3 320 - 335 °C
608 - 635 °F
C3 Cylinder Temp for Electronic and Electric Standard Molding
325 - 340 °C
617 - 644 °F
C3 Cylinder Temp for Mechanical and Structural Standard Molding
Mold Temperature 50.0 - 90.0 °C
122 - 194 °F
for Mechanical and Structural Standard Molding
90.0 - 140 °C
194 - 284 °F
for Electronic and Electric Standard Molding
Screw Speed 150 rpm
150 rpm
for Mechanical and Structural Standard Molding
150 rpm
150 rpm
for Electronic and Electric Standard Molding
Descriptive Properties Value Comments
Injection Pressure Medium
Electronic and Electric Standard Molding
Medium
Mechanical and Structural Standard Molding
Injection Speed Medium
Electronic and Electric Standard Molding
Medium
Mechanical and Structural Standard Molding