Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Graphite Filled
Manufacturer Ensinger
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal stability. The bearing grades of the XP 150 Series have excellent wear because of the encapsulated graphite used.The XP 150 Series of Polyimides are non-melting high temperature materials with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.Typical Applications:Bearings and BushingsBall Valve SeatsSemiconductor Processing EquipmentGearsTanksElectrical ComponentsPump PartsHydraulic ComponentsGasketsCircuit BoardsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Filler Content 15 %
15 %
Mechanical Properties Metric English Comments
Tensile Strength 59.3 MPa
8600 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Tensile Modulus 5.03 GPa
730 ksi
ASTM D638
Flexural Strength 101 MPa
14700 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790