| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded |
| Manufacturer | Mitsubishi |
| Trade Name | Xantar® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Mitsubishi Xantar® 24 UR Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Water Absorption | 0.35 % | 0.35 % | Sim. to ISO 62 |
| Viscosity Test | 52 cm³/g | 52 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
| 58 cm³/g | 58 cm³/g | Viscosity Number | |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
| Melt Flow | 8.4 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
8.4 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
Calculated from Volume Flow Rate of 7 cm<sup>3</sup>/10min.; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ISO 2039-2 |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | ISO 527-1/-2 |
| Elongation at Break | >= 50 % | >= 50 % | ISO 527-1/-2 |
| Elongation at Yield | 6.0 % | 6.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1/-2 |
| Flexural Strength | 90.0 MPa | 13100 psi | ISO 178 |
| Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 80.0 kJ/m² <br>@Temperature 23.0 °C |
38.1 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180/4A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 65.0 µm/m-°C <br>@Temperature 20.0 °C |
36.1 µin/in-°F <br>@Temperature 68.0 °F |
ISO 11359-1/-2 |
| Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °C | 266 °F | ISO 75-1/-2 |
| Vicat Softening Point | 150 °C | 302 °F | 50°C/h 50N; ISO 306 |
| UL RTI, Electrical | 130 °C <br>@Thickness 0.750 mm |
266 °F <br>@Thickness 0.0295 in |
UL746B |
| 130 °C <br>@Thickness 3.00 mm |
266 °F <br>@Thickness 0.118 in |
UL746B | |
| UL RTI, Mechanical with Impact | 125 °C <br>@Thickness 0.750 mm |
257 °F <br>@Thickness 0.0295 in |
UL746B |
| 130 °C <br>@Thickness 3.00 mm |
266 °F <br>@Thickness 0.118 in |
UL746B | |
| UL RTI, Mechanical without Impact | 125 °C <br>@Thickness 0.750 mm |
257 °F <br>@Thickness 0.0295 in |
UL746B |
| 130 °C <br>@Thickness 3.00 mm |
266 °F <br>@Thickness 0.118 in |
UL746B | |
| Flammability, UL94 | V-2 <br>@Thickness 0.750 mm |
V-2 <br>@Thickness 0.0295 in |
IEC 60695-11-10 |
| V-2 <br>@Thickness 1.60 mm |
V-2 <br>@Thickness 0.0630 in |
IEC 60695-11-10 | |
| Oxygen Index | 26 % | 26 % | ISO 4589-1/-2 |
| Glow Wire Test | 800 °C <br>@Thickness 1.50 mm |
1470 °F <br>@Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| 825 °C <br>@Thickness 1.50 mm |
1520 °F <br>@Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 | |
| 875 °C <br>@Thickness 3.00 mm |
1610 °F <br>@Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 | |
| 960 °C <br>@Thickness 3.00 mm |
1760 °F <br>@Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 89 % | 89 % | Light Transmittance; ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 2.9 <br>@Frequency 1e+6 Hz |
2.9 <br>@Frequency 1e+6 Hz |
IEC 60250 |
| 3.0 <br>@Frequency 100 Hz |
3.0 <br>@Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.00066 <br>@Frequency 100 Hz |
0.00066 <br>@Frequency 100 Hz |
IEC 60250 |
| 0.0092 <br>@Frequency 1e+6 Hz |
0.0092 <br>@Frequency 1e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Blow Molding | Yes | |
| Heat stabilized or stable to heat | Yes | |
| High impact or impact modified | Yes | |
| Injection molding | Yes | |
| Light stabilized or stable to light | Yes | |
| Release Agent | Yes | |
| Transparent | Yes | |
| U.V. stabilized or stable to weather | Yes | |
| Without Fillers | Yes |