| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1A |
| Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
63.5*12.7*3.2; ISO 180/4A |
| SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
63.5*12.7*3.2; ISO 180/4A |
| SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
| Izod Impact, Notched (ISO) | 80.0 - 90.0 kJ/m² | 38.1 - 42.8 ft-lb/in² | Average value: 82.5 kJ/m² Grade Count:4 |
| Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 24 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180-1A |
| Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® FC 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® MX 2015 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYL® A 246M PA66, Conditioned Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYL® C 206 PA6, Conditioned Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ASTM D256 |
| Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ASTM D256 |
| Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Thickness >=5.00 mm |
38.1 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
| Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/4A |
| Chi Mei Wonderlite® PC-110U Polycarbonate - UV Stabilized UV Stabilized |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/4A |
| Chi Mei Wonderlite® PC-110V Polycarbonate - Flame Retardant |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | ISO 180/4A |
| Chi Mei Wonderlite® PC-110N Polycarbonate - Flame Retardant Opaque |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Eurotec® Tecomid® NB50 BK001 IH PA6, impact modified, black, extrusion grade Information provided by Eurotec® |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
| Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
| Izod Impact, Notched (ISO) | 80.0 kJ/m² | 38.1 ft-lb/in² | 50%RH; Partial; ISO 180/1A |
| DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |
|||